Test results of physical properties of SMA-13 aggregates.

Items10∼15 mm5∼10 mm3∼5 mm0∼3 mmMineral powderRequirements

Apparent relative density2.9232.9132.862≥2.6
2.8182.756≥2.5
Volume relative density2.8702.863
Water absorption (%)0.630.60≤2
Crushing value (%)10.5≤20
Wear value (%)12.4≤28