Ultimate strain of steel wire under uniform corrosion.

Corrosion time (h)Corrosion length (mm)Corrosion depth (mm)Ultimate strainCorrosion time (h)Corrosion length (mm)Corrosion depth (mm)Ultimate strain

1001.250.0080.0465001.250.0420.041
2.500.0080.0452.500.0420.038
3.750.0080.0443.750.0420.037
5.000.0080.0445.000.0420.033

2001.250.0170.0456001.250.050.039
2.500.0170.0442.500.050.036
3.750.0170.0433.750.050.034
5.000.0170.0425.000.050.031

3001.250.0250.0437001.250.0590.037
2.500.0250.0422.500.0590.034
3.750.0250.0413.750.0590.032
5.000.0250.0385.000.0590.029

4001.250.0340.0438001.250.0670.036
2.500.0340.042.500.0670.033
3.750.0340.0383.750.0670.031
5.000.0340.0365.000.0670.027