Research Article
Thermal Analysis of Ni-Cu Alloy Nanocomposites Processed by Sand Mold Casting
Table 13
CTE of the Ni-Cu alloy + 12% TiO2 composite.
| Specimen length (mm) | Specimen temperature | Delta T | Rod elongation (mm) | Delta L (mm) | Coefficient of thermal expansion |
| 50 | 100 | 0 | 0.001 | 0 | 0 | 50 | 125 | 22 | 0.009 | 0.003 | 2 × 10−6 | 50 | 150 | 25 | 0.017 | 0.005 | 4 × 10−6 | 50 | 175 | 25 | 0.021 | 0.006 | 7 × 10−6 | 50 | 200 | 25 | 0.036 | 0.011 | 10 × 10−6 | 50 | 225 | 25 | 0.042 | 0.012 | 11 × 10−6 | 50 | 250 | 25 | 0.046 | 0.013 | 12 × 10−6 | 50 | 275 | 25 | 0.048 | 0.014 | 13 × 10−6 | 50 | 300 | 25 | 0.051 | 0.015 | 14 × 10−6 | 50 | 325 | 25 | 0.054 | 0.016 | 15 × 10−6 | 50 | 350 | 25 | 0.059 | 0.017 | 16 × 10−6 |
|
|