Mix design for normal strength concrete.

CMWGSSPAEAW/cmCompressive strength (MPa)References

41520810497290.04150.5050[119]
3901561297.8566.21.950.4050[120]
3201601286.4633.61.920.5040
2801681249.3702.71.680.6030
40020093087340.5040[121]