Advances in Materials Science and Engineering / 2022 / Article / Tab 8 / Research Article
Experimental Investigation and Optimization of Material Removal Rate and Tool Wear in the Machining of Aluminum-Boron Carbide (Al-B4 C) Nanocomposite Using EDM Process Table 8 MRR and TWR obtained during EDM of Al-B4 C.
S. no. Tool diameter (mm) Current (amps) On-time (micro sec) Wt. of W/P before (gm) Wt. of W/P after (gm) Wt. of tool before (gm) Wt. of tool after (gm) MRR (m3 /min) TWR (m3 /min) 1 4 1 4 118.69 118.08 9.27 9.25 0.061 0.002 2 4 2 3 118.08 117.59 9.25 9.23 0.049 0.002 3 4 3 1 117.59 117.07 9.23 9.21 0.052 0.003 4 4 4 2 117.07 116.56 9.21 9.19 0.051 0.002 5 6 1 3 116.56 115.50 11.38 11.36 0.10 0.002 6 6 2 4 115.50 114.52 11.36 11.33 0.098 0.003 7 6 3 1 114.52 113.51 11.33 11.31 0.10 0.002 8 6 4 2 113.51 112.50 11.31 11.28 0.10 0.003 9 8 1 4 112.50 110.98 14.16 14.12 0.15 0.004 10 8 2 3 110.98 109.49 14.12 14.09 0.14 0.003 11 8 3 2 109.49 108.97 14.09 14.05 0.052 0.004 12 8 4 1 108.97 107.50 14.05 14.01 0.14 0.004 13 10 1 2 107.50 105.82 36.25 36.22 0.16 0.003 14 10 2 1 105.82 103.72 36.22 36.18 0.21 0.004 15 10 3 3 103.72 101.32 36.18 36.14 0.24 0.004 16 10 4 4 101.32 98.91 36.14 36.10 0.24 0.004