Research Article

Calibration of Contact Parameters for Moist Bulk of Shotcrete Based on EDEM

Table 5

Results of steepest ascent test.

No.T2T7T3Repose angle (°)Relative error (%)

10.010.010.0111.0672.35
20.20.10.0229.1227.2
30.40.20.0431.3421.65
40.60.30.0636.259.375
50.80.40.0839.162.1
610.50.142.446.1