Research Article
Role of Cobalt Doping on the Physical Properties of CdO Nanocrystalline Thin Films for Optoelectronic Applications
Table 3
NLO parameters of Cd1 − xCoxO thin films.
| Composition of Co (X) | NLA | NRI () ×10−8 (cm2/W) | Real part of NLO susceptibility (χ(3) R) ×10−7 (esu) | Imaginary part of NLO susceptibility ×10−7 (χ(3) img) esu | Third order NLO susceptibility (χ3) |
| Wt.% | Coefficient (β) ×10−3 (cm/W) | 5.33 | 6.78 | Davg | (Esu) | Pure CdO | 0.92 | −1.35 | 7.53 | 3.19 | 7.62 × 10−7 | 1% Co | 1.35 | −1.48 | 8.06 | 3.26 | 8.32 × 10−7 | 5% Co | 3.64 | −1.68 | 9.12 | 4.46 | 9.36 × 10−7 | 10% Co | 6.18 | −1.86 | 9.85 | 5.62 | 1.42 × 10−6 |
|
|