Response table for means (wear test).

Level% of reinforcementStir speed (rpm)Stir time (min)Molten temperature (oC)

10.28460.21090.27130.2360
20.27320.27800.28590.3190
30.19500.26390.19560.1978
Delta0.12120.08960.09030.0671
Rank1324