Research Article
Research on the Creep and Fatigue Evaluation Method of the Double-Layered Annulus Metal Hydride Bed Combined with Numerical Modeling and ASME Code
Table 6
Evaluation results of thermal fatigue and creep.
| Evaluation item | C-C | D-D | Calculated value | Limit | Check | Calculated value | Limit | Check |
| Primary stress limits (MPa) | Membrane | 3.22 | 106 | Ok | 5.93 | 106 | Ok | Membrane + bending | 5.24 | 167 | Ok | 9.80 | 167 | Ok |
| Inelastic strain limits | Elastic analysis | 0.732 | 1.0 | Ok | 0.542 | 1 | Ok | Simplified inelastic analysis | 0.000 | 1% | Ok | 0.000 | 1% | Ok |
| Creep-fatigue limits | Fatigue damage | 0.084 | — | — | 0.016 | — | — | Creep damage | 0.1 | — | — | 0.1 | — | — |
|
|