Research Article
Optimizing the Parameters of Spark Plasma Sintering to Enhance the Hardness of MgO/TiC Composites
Table 1
Design of Taguchi
orthogonal arrays.
| Specimen | Sintering temperature | Sintering pressure | Sintering time | (°C) | (MPa) | (min) |
| 1 | 500 | 35 | 15 | 2 | 500 | 45 | 20 | 3 | 500 | 55 | 25 | 4 | 550 | 35 | 20 | 5 | 550 | 45 | 25 | 6 | 550 | 55 | 15 | 7 | 600 | 35 | 25 | 8 | 600 | 45 | 15 | 9 | 600 | 55 | 20 |
|
|