Clay analysis results of the three experiments (XRD).

Test nameClay contents (%)
SmectiteI/SIlliteKaoliniteChlorite

scCO2 test33.54.119.216.127.1
32.26.221.314.525.8
28.44.521.016.829.3
342.720.415.227.7
31.34.821.116.426.4
32.92.719.616.927.9
32.22.820.516.128.4

N2 test22.82.531.717.225.8
23.13.229.218.326.2
23.42.130.117.926.5
24.62.432.415.724.9
24.44.529.316.725.1
25.51.728.516.927.4
26.33.330.115.924.5

Helium test24.53.429.316.126.7
25.82.031.814.625.8
26.14.629.715.723.9
25.93.727.516.226.7
23.71.431.217.426.3
25.42.629.816.825.4
22.81.631.615.928.1