Research Article

Effect of Hot Rolling on Friction and Wear Characteristics of TiC Reinforced Copper-Based Metal Matrix Composites

Figure 14

SEM of worn-out surfaces of the cast and rolled alloy and composites at different sliding velocities: (a) 0.628 m/s, (b) 0.628 m/s, (c) 2.512 m/s, (d) 2.512 m/s, (e) 0.628 m/s, (f) 0.628 m/s, (g) 2.512 m/s, and (h) 2.512 m/s.