Research Article
Steel Pipe Internal Corrosion Protection Using Magnesium Anode: Impact of Protective Potential and Phase Layer Formation on Corrosion Rate
Table 2
Water parameters in tap water depending on the test conditions.
| No. | Conditions | TDS (mg/L) | Calcium hardness (mg/L) | Total alkalinity (mg/L) | Water temperature (°C) | pH | pHs | LI |
| 1 | Fresh water | 220 | 200 | 100 | 45 | 8.20 | 6.9 | 1.3 | 2 | Blank experiment | 160 | 100 | 50 | 45 | 8.90 | 7.5 | 1.4 | 3 | Magnesium dissolution | 290 | 100 | 200 | 45 | 9.20 | 6.9 | 2.3 |
|
|