Research Article
Optimization of Wear Process Parameters of Al6061-Zircon Composites Using Taguchi Method
Figure 2
SEM images of Al6061 alloy and Al6061-Zircon composite specimens at 500x magnifications for different wt. % of Zircon, (a) Al6061 at 500x (b) Al6061 + 3% Zircon at 500x, (c) Al6061 + 6% Zircon at 500x (d) Al6061 + 9% Zircon at 500x, and (e) Al6061 + 12% Zircon at 500x.
(a) |
(b) |
(c) |
(d) |
(e) |