ANOVA table for delamination factor.
| At the entry | At the exit | Source | Degree of freedom | value | value | Degree of freedom | value | value |
| Model | 15 | 47.75 | 0.001 | 6 | 13.56 | 0.001 | Linear | 6 | 20.90 | 0.001 | 6 | 13.56 | 0.001 | Spindle speed () | 2 | 4.70 | 0.045 | 2 | 23.18 | 0.001 | Feed rate () | 1 | 0.35 | 0.573 | 1 | 2.46 | 0.135 | Coating thickness () | 3 | 38.55 | 0.001 | 3 | 10.86 | 0.001 | 2-way interactions | 9 | 65.66 | 0.001 | — | — | — | | 6 | 91.53 | 0.001 | — | — | — | | 3 | 13.92 | 0.002 | — | — | — | Error | 8 | — | — | 17 | — | — | Total | 23 | — | — | 23 | — | — | Standard deviation | 0.0062452 | 0.0189956 | -square | 98.90% | 82.72% | -square (adjusted) | 96.82% | 76.62% | -square (predicted) | 90.06% | 65.56% |
|
|