Density values of the sintered mixtures.

Sintering temperatureDwell timeDensity
Alloy 1Alloy 2Alloy 3

800206.816.686.59
356.876.726.54
506.856.86.71

850206.796.586.56
356.846.616.55
506.836.676.57

900206.726.546.54
356.766.536.52
506.736.546.53