Research Article
Wear Behavior and Its Correlation with Mechanical Properties of TiB2 Reinforced Aluminium-Based Composites
Table 1
Data of tensile test conducted on cast Al, Al-MMCs and gray cast iron.
| Sr. no. | Properties | Pure aluminium | Al-2.5%TiB2 | Al-5%TiB2 | Gray cast iron |
| 1 | Y.S (MPa) | 74 | 93 | 96 | ā | 2 | UTS (MPa) | 121 | 157 | 180 | 284 | 3 | Fracture strength (MPa) | 70 | 78 | 150 | 284 | 5 | %Reduction in area | 22.53 | 16.84 | 9.38 | 3.19 | 6 | %Elongation | 8 | 6.5 | 6 | 3 |
|
|