Research Article

Structure and Abrasive Wear of Composite HSS M2/WC Coating

Figure 8

Abrasive wear rate versus WC content in the source powder mixture. (a) Quartz sand, ((b), (c), (d)) electrocorundum; (a), (b) just after cladding; (c) single tempering; (d) double tempering.
502714.fig.008a
(a)
502714.fig.008b
(b)
502714.fig.008c
(c)
502714.fig.008d
(d)