Research Article

Surface Layer Properties after Successive EDM or EDA and Then Superficial Roto-Peen Machining

Figure 11

SEM surface layer image after the alloying with the electrode of alloy steel 1H18N9 (I = 32 A, Ti = 25 μs); measuring points (Table 2) have been marked.
723919.fig.0011