Research Article

Surface Layer Properties after Successive EDM or EDA and Then Superficial Roto-Peen Machining

Table 2

Specification of the chemical composition investigation results for the surface layer after the alloy steel 1H18N9 electrode alloying; pulse current I = 32 (A), pulse Ti = 25 (μs), electrode material: 1H18N9.

18LSi-KCr-KMn-KNi-K

pt10.395.911.092.64
pt20.355.471.382.60
pt30.373.591.142.02
pt40.334.851.331.40
pt50.380.500.920.00
pt60.250.380.510.16
pt70.280.290.750.15
pt80.420.091.200.44
pt90.360.240.630.53
pt100.350.191.050.04