Research Article
Experimental Evaluation of Erosion of Gunmetal under Asymmetrical Shaped Sand Particle
Figure 19
SEM micrograph of eroded aluminum alloy at impact angle, (a, b) 15 degrees, (c, d) 30 degrees, and (e, f) 60 degrees.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |