Research Article

Processing and Wear Behaviour of 3D Printed PLA Reinforced with Biogenic Carbon

Table 3

Results from Raman spectroscopy, 532 nm laser wave length.

sample D-peak positionG-peak positionIntensity ratio //nm

biocarbon 11345.91595.60.912.331

biocarbon 21340.01596.10.892.363

biocarbon 31338.01595.30.912.375

biocarbon 41340.01599.00.882.375

mean value1341.01596.50.902.350

standard deviation3.41.70.020.02

: in-plane crystallite size after pyrolysis at 800°C.