Journals
Publish with us
Publishing partnerships
About us
Blog
International Journal of Analytical Chemistry
Journal overview
For authors
For reviewers
For editors
Table of Contents
Special Issues
International Journal of Analytical Chemistry
/
2017
/
Article
/
Tab 2
/
Research Article
Formulation Development of High Strength Gel System and Evaluation on Profile Control Performance for High Salinity and Low Permeability Fractured Reservoir
Table 2
The gelling performance of the ABP system at different salinities.
Formulation
Delayed crosslinking time
(days)
Gel strength (mPa·s)
Initial viscosity (mPa·s)
Stability (days)
Temperature (°C)
Polymer P (mg/L)
Crosslinking agent A
(%)
Coagulant B (%)
Salinity (mg/L)
32
3500
0.3
0.09
15000
2-3
>20000
110.7
>60
29500
5-6
>14500
33.0
>60
45000
7-8
>10500
21.2
>60