Research Article

Preparation and Anticorrosion of Octadecyl Trichlorosilane SAMs for Copper Surface

Table 1

The fitting parameters of polarization of copper and copper SAMs in 1 mol/L HCl solution.

Inhibitor concentration/ppm (V) (μA/cm2) (V) (V)

Blank3.18 × 1030.0600.039
100.181340.1120.056
200.33760.1010.003
300.452.30.0850.054
400.570.590.0250.056