Research Article

Studies on the Process Parameters of Rapid Prototyping Technique (Stereolithography) for the Betterment of Part Quality

Table 2

L9 orthogonal array.

Experimental run ()Levels
ABC
Layer thickness ()—mmOrientation ()—°Hatch spacing ()—mm

1111
2122
3133
4212
5223
6231
7313
8321
9332