Summary of analytical data.

Iron loading concentration (mol%)SSA (m2/g) (eV)BET diameter (nm)

0130.003.216.39
0.50134.002.956.20
1.00137.972.706.02
1.50137.992.656.02
2.00139.002.555.98
5.00140.822.455.57
10.00148.762.355.27