Controlled Morphology and Mechanical Characterisation of Electrospun Cellulose Acetate Fibre Webs
Figure 10
SEM images of the surface of the regenerated cellulose fibres at a polymer concentration of 25% (w/v). The operating voltage was 25 kV and the flow rate 0.002 (mL min−1).