Microwave Synthesized Monodisperse CdS Spheres of Different Size and Color for Solar Cell Applications

Figure 5

XRD patterns of CdS products synthesized (a) at 100 and 150°C for 10 min from solutions of pH 8.4–8.5 (Figures 5(a) and 5(b), resp.), (b) at 100°C and 150°C for 10 min from solutions of pH 11.0–11.3 (Figures 4(a) and 4(c), resp.).
(a) pH 8.4–8.5
(b) pH 11.0–11.3