Research Article

Ultrasound-Assisted Rapid ZIF-8 Synthesis, Porous ZnO Preparation by Heating ZIF-8, and Their Photocatalytic Activity

Figure 10

Photocatalytic decomposition of MB on Z--(3 h) samples, with , 500, or 660°C (experimental conditions: 0.5 g/L catalyst; MB 5 mg/L; 30°C; UV irradiation after 60 minutes).