Research Article
Ultrasound-Assisted Rapid ZIF-8 Synthesis, Porous ZnO Preparation by Heating ZIF-8, and Their Photocatalytic Activity
Table 1
Porous properties of ZIF-8 samples.
| Sample | BET surface area (m2·g-1) | -Plot micropore area (m2·g-1) | -Plot external surface area (m2·g-1) | -Plot micropore volume (cm3·g-1) |
| Z-stir-(8 h) | 1279 | 1237 | 42 | 0.604 | Z-ultrasound-(0.5 h) | 1367 | 1324.5 | 42.5 | 0.633 |
|
|