Research Article

Wear Characteristic of Stellite 6 Alloy Hardfacing Layer by Plasma Arc Surfacing Processes

Figure 6

SEM images of Stellite 6 after friction tests at room temperature under (a) 10 N and (b) 15 N applied loadings and at 300°C under (c) 10 N and (d) 15 N applied loadings. (e) EDS analysis of Figure 6(c) and (f) EDS analysis of Figure 6(d).
(a)
(b)
(c)
(d)
(e)
(f)