Comparison of the best WSP coating of WC-Co (115–300) with other materials studied by the authors under the same conditions.

MATERIALSAR—wear coef. [ /Nm]DSRW—wear coef. [m /Nm]Microhardness [GPa]

WC-17Co (115–300)0.000100.00017
WC-17Co, HVOF0.000020.00009
, WSP-sprayed0.000100.00113
Hard chrome0.000190.00056