Research Article

Tribological Analysis of Particulates Reinforced Powder Metallurgy Magnesium Alloy Composites under Oil Lubrication Condition

Figure 8

Sliding surfaces of pin specimens (upper) and AZ31B disks (lower) when employing Mg-Y-Zn alloy composite reinforced with 5 wt%   particles via RPW process with (a) 200, (b) 400 and (c) 600 cycles.
628737.fig.008a
(a) 5% (N = 200)
628737.fig.008b
(b) 5% (N = 400)
628737.fig.008c
(c) 5% (N = 600)