Research Article

Laser Beam Welding of AA5052, AA5083, and AA6061 Aluminum Alloys

Figure 2

Face side (a) and root side (b) of alloy AA5083 welded using P = 4 kW, S = 6 m/min, Dd = 0, 15 l/min argon.
974182.fig.002a
(a)
974182.fig.002b
(b)