Review Article
Recent Advances in the Deposition of Diamond Coatings on Co-Cemented Tungsten Carbides
Table 3
Cracks radius on diamond coatings after laser (1250 W) and MP treatments.
| Load | Crack radius, m | After laser treatment at 1250 W | After MP treatment |
| 28 kg | 195 ± 23 | 204 ± 29 | 45 kg | 253 ± 31 | 239 ± 28 | 62 kg | 290 ± 30 | 308 ± 36 | 105 kg | 388 ± 59 | 370 ± 38 | 154 kg | 483 ± 41 | 495 ± 46 |
| | (dX/dP)−1, m/kg |
| | 0.437 ± 0.03 | 0.452 ± 0.04 |
|
|