Research Article
Durability Index Performance of High Strength Concretes Made Based on Different Standard Portland Cements
Table 1
Mixtures for the various concretes.
| |
Cements: CEM I 42.5N, CEM II/A-V52.5N, CEM IV/B-V 32.5R, CEM II/A-M (V-L) | Cements: CEM I 42.5N FS, CEM II/A-V 52.5N FS | | w/c = 0.65 | w/c = 0.5 | w/c = 0.4 | w/c = 0.5 |
| Cement (kg) | 6.4 | 7.6 | 8.7 | 7.6 | Water (kg) | 4.2 | 3.8 | 3.5 | 3.8 | 19 mm dolomite stone (kg) | 20.3 | 20.3 | 20.3 | 20.3 | Dolomite crusher sand (kg) | 16.0 | 16.0 | 16.0 | 13 | Filler sand (kg) | 0 | 0 | 0 | 3.2 | Admixture Chryso 209 (mls) | 0 | 0 | 40 | 0 |
|
|