Research Article

Flexural Behavior of Extruded DFRCC Panel and Reinforced Concrete Composite Slab

Table 4

Experimental results for DFRCC panel specimens.

Name (MPa) (mm) (MPa) (mm) / Stiffness (kN/mm)No. of cracks

DFRCC29.10.67537.06.119.0142.112

fi: flexural strength at initial crack, : midspan deflection at fi, : maximum flexural strength, : midspan deflection at f.