Research Article

Experimental Research on Fire Resistance of Reactive Powder Concrete

Table 3

Observations of two types of RPC with various moisture contents after spalling tests.

Moisture content0.16S2.00.18P0.10S2.0
ObservationBrief descriptionObservationBrief description

100%860303.tab.001aA cube fully spalled and broke into small pieces.860303.tab.001bA cube fully spalled and broke into small pieces.
88%860303.tab.001cA cube fully spalled and broke into small pieces.860303.tab.001dA cube fully spalled and broke into small pieces.
75%860303.tab.001eA cube fully spalled and broke into small pieces.860303.tab.001fA cube spalled and broke into small and large pieces.
63%860303.tab.001gA cube fully spalled and broke into small or large pieces.860303.tab.001hA cube partially spalled.
50%860303.tab.001iA cube fully spalled and broke into large pieces.860303.tab.001jA cube partially spalled.
25%860303.tab.001k A cube fully spalled and broke into large pieces.860303.tab.001lA cube with minor spalling.
860303.tab.001mA cube remained intact (no spalling).
0%860303.tab.001nA cube partially spalled.860303.tab.001oA cube remained intact (no spalling).