Performance Comparison between Neutralization Tailings and Flotation Tailings Used for Backfill Mix and Mechanism Analysis
Table 2
The results of the first experiment.
| Number | Slump (mm) | Diffusivity (mm) | UCS (MPa) | Number | Slump (mm) | Diffusivity (mm) | UCS (MPa) | 7 d | 14 d | 28 d | 7 d | 14 d | 28 d |
| A1 | 175 | 320 | 1.43 | 3.07 | 3.63 | A11 | 140 | 220 | 3.1 | 4.67 | 5.54 | A2 | 250 | 530 | 1.17 | 2.56 | 3.55 | A12 | 265 | 620 | 3.7 | 6.01 | 7.19 | A3 | 265 | 770 | 1.13 | 2.81 | 3.71 | A13 | 280 | 870 | 2.6 | 4.37 | 6.50 | A4 | 275 | 1090 | 1.37 | 2.88 | 3.93 | A14 | 285 | 1025 | 1.9 | 2.70 | 3.79 | A5 | 280 | 1140 | 1.57 | 2.87 | 4.22 | A15 | 285 | 845 | 2.1 | 2.60 | 4.19 | A6 | 160 | 280 | 0.77 | 1.24 | 1.74 | A16 | 140 | 268 | 1.33 | 2.24 | 3.53 | A7 | 265 | 735 | 0.67 | 1.12 | 1.36 | A17 | 255 | 503 | 1.20 | 2.41 | 2.70 | A8 | 270 | 825 | 0.57 | 1.00 | 1.51 | A18 | 283 | 850 | 1.07 | 1.49 | 2.07 | A9 | 273 | 865 | 0.56 | 1.11 | 1.47 | A19 | 278 | 885 | 0.84 | 1.23 | 1.77 | A10 | 260 | 960 | 0.68 | 1.18 | 1.66 | A20 | 288 | 1035 | 0.71 | 1.09 | 1.60 |
|
|