Research Article
Improved Reactivity of Fly Ash-Slag Geopolymer by the Addition of Silica Fume
Table 2
Mix proportion of fly ash-slag geopolymer paste.
| Sample | Water/binder | AA/water | SF/(FA + BFS + SF) | FA/BFS |
| C | 0.38 | 0.20 | 0 | 1.0 | SF1-10 | 0.38 | 0.20 | 0.10 | 0.8 | SF1-20 | 0.38 | 0.20 | 0.20 | 0.6 | Z10 | 0.38 | 0.20 | 0.10 | 0.8 | HFA | 0.38 | 0.20 | 0 | 1.0 | SF1-10S | 0.38 | 0.20 | 0.10 | 1.25 | SF1-20S | 0.38 | 0.20 | 0.20 | 1.67 | Z10S | 0.38 | 0.20 | 0.10 | 1.25 | SF2-10 | 0.38 | 0.20 | 0.10 | 0.8 | SF2-20 | 0.38 | 0.20 | 0.20 | 0.6 | SF2-10S | 0.38 | 0.20 | 0.10 | 1.25 | SF2-20S | 0.38 | 0.20 | 0.20 | 1.67 |
|
|
AA indicates the alkaline activator with SiO2/Na2O ratio of 0.97.
|