Calculated fraction of FCC Copper precipitates and Copper atoms in the solid solution in 18CrNiMo7-6 carburizing steel with different heat treatment conditions.

FCC CuCu in solid solution

1.5% Cu, aged at 500°C for 21600 s0.5640.436
1.5% Cu, aged at 500°C for 10000 s0.4590.541
1.0% Cu, aged at 480°C for 14400 s0.2820.718
1.0% Cu, aged at 480°C for 3000 s0.1730.827

Can be inaccurate as coherent BCC Cu precipitates are expected.