Research Article
Fabrication of SiC Composites with Synergistic Toughening of Carbon Whisker and In Situ 3C-SiC Nanowire
Table 1
Mechanical properties of hot-press sinter and annealed specimen of
/SiC composites.
| Material | Relative density | Flexure strength (MPa) | Fracture toughness (MPa⋅m1/2) |
| HPM | 99.1% | 235 ± 6.1 | 5.21 ± 0.34 | AM10 | 98.9% | 241 ± 4.7 | 5.24 ± 0.32 | AM30 | 98.5% | 246 ± 5.5 | 5.35 ± 0.19 | AM60 | 98.4% | 294 ± 4.2 | 6.43 ± 0.36 | AM90 | 98.1% | 278 ± 2.9 | 5.59 ± 0.27 |
|
|