Test results of autogenous shrinkage of SFRLAC.
| Mix number | Curing age (days) | 1 | 3 | 7 | 14 | 28 | 60 | 90 | 120 | 150 | 180 | 210 | 240 | 270 |
| HL0.25/0.8 | 0 | 27 | 72 | 116 | 152 | 170 | 180 | 182 | 182 | 182 | 183 | 183 | 183 | HL0.30/0.8 | 0 | 19 | 48 | 84 | 123 | 144 | 159 | 161 | 161 | 162 | 162 | 162 | 162 | HL0.35/0.8 | 0 | 15 | 38 | 68 | 112 | 132 | 141 | 149 | 150 | 150 | 150 | 150 | 150 | NL0.30/0.8 | 0 | 72 | 115 | 146 | 152 | 162 | 164 | 170 | 170 | 171 | 171 | 172 | 172 | HM0.30/0.8 | 0 | 44 | 56 | 69 | 92 | 104 | 118 | 122 | 124 | 126 | 130 | 133 | 134 | NM0.30/0.8 | 0 | 44 | 62 | 67 | 98 | 121 | 134 | 140 | 140 | 141 | 142 | 142 | 142 |
|
|