Effects of High Magnetic Field Postannealing on Microstructure and Properties of Pulse Electrodeposited Co-Ni-P Films

Figure 4

The in-plane hysteresis loops of as-deposited Co-Ni-P film and of the films annealed at 673 K for 4 h under 0 T, 6 T, and 12 T magnetic field conditions.