Research Article

Combating Wear of ASTM A36 Steel by Surface Modification Using Thermally Sprayed Cermet Coatings

Figure 6

Variation of C.W.R. for uncoated and D-Gun spray coated ASTM A36 steel at normal applied load of (a) 40 N; (b) 50 N; (c) 60 N at sliding velocity of 2 ms−1.
(a)
(b)
(c)