Numerical Simulation of Recycled Concrete Using Convex Aggregate Model and Base Force Element Method

Table 3

The average uniaxial compressive strength of different sizes of RAC specimens.

Dimensions of RACMeans of compressive strength/MPa

100 mm × 100 mm26.15
150 mm × 150 mm25.15
300 mm × 300 mm23.56