Research Article
Effect of Polypropylene and Basalt Fiber on the Behavior of Mortars for Repair Applications
Table 4
Mix proportions of the mortar.
| Mix | Cement (kg/m3) | Sand (kg/m3) | Water (kg/m3) | PP fiber (kg/m3) | BF (kg/m3) | Superplasticizer (%) |
| Control | 680.8 | 1361.6 | 367.3 | — | — | 0.2 | PP-0.6 | 680.8 | 1361.6 | 367.3 | 0.6 | — | 0.2 | PP-1.6 | 680.8 | 1361.6 | 367.3 | 1.6 | — | 0.2 | PP-2.6 | 680.8 | 1361.6 | 367.3 | 2.6 | — | 0.2 | BF-0.6 | 680.8 | 1361.6 | 367.3 | — | 0.6 | 0.2 | BF-1.6 | 680.8 | 1361.6 | 367.3 | — | 1.6 | 0.2 | BF-2.6 | 680.8 | 1361.6 | 367.3 | — | 2.6 | 0.2 |
|
|