Weight loss of the mortar specimens after the freeze-thaw cycles.
| Repair mortar | Weight loss (%) | 50 cycles | 100 cycles | 150 cycles |
| Control | 0.25 | 0.56 | 0.92 | PP-0.6 | 0.16 | 0.39 | 0.78 | PP-1.6 | 0.12 | 0.32 | 0.73 | PP-2.6 | 0.09 | 0.27 | 0.68 | BF-0.6 | 0.19 | 0.46 | 0.86 | BF-1.6 | 0.16 | 0.40 | 0.81 | BF-2.6 | 0.14 | 0.36 | 0.76 |
|
|