Research Article
Urea Formaldehyde Composites Reinforced with Sago Fibres Analysis by FTIR, TGA, and DSC
Table 1
Results for Sago/UF Sample with different particle size analysis by TGA.
| Size | Temperature range | Temperature peak | Weight loss | Residue | (°C) | (°C) | (%) | (%) |
| Sample A | 62–161 | 75 | 3 | 27 | 0.6 mm | 184–539 | 312 | 71 | Sample B | 55–168 | 82 | 2 | 25 | 1.18 mm | 176–574 | 311 | 73 | Sample C | 55–175 | 86 | 9 | 15 | 2 mm | 193–585 | 311 | 76 |
|
|