Thermochemical Properties of Glass Wool/Maerogel Composites
Table 1
The different loaded Maerogels.
| ā | Case | Case | Case | Case | Case |
| Weight% | 0 | 5.4 | 10.2 | 14.6 | 18.6 | Loaded Maerogel (gr)/total weight after drying (gr) | 0 | 0.054 | 0.102 | 0.14 | 0.186 |
|
|